1.1 ,This method describes the analysis of titanium and titanium alloys, such as specified by committee B10, by inductively coupled plasma atomic emission spectrometry (ICP-AES) and direct current plasma atomic emission spectrometry (DCP-AES) for the following elements:
| Element | Application | Quantitative |
| Aluminum | 0–,8 | 0.009 to 8.0 |
| Boron | 0–,0.04 | 0.0008 to 0.01 |
| Cobalt | 0-1 | 0.006 to 0.1 |
| Chromium | 0–,5 | 0.005 to 4.0 |
| Copper | 0–,0.6 | 0.004 to 0.5 |
| Iron | 0–,3 | 0.004 to 3.0 |
| Manganese | 0–,0.04 | 0.003 to 0.01 |
| Molybdenum | 0–,8 | 0.004 to 6.0 |
| Nickel | 0–,1 | 0.001 to 1.0 |
| Niobium | 0-6 | 0.008 to 0.1 |
| Palladium | 0-0.3 | 0.02 to 0.20 |
| Ruthenium | 0-0.5 | 0.004 to 0.10 |
| Silicon | 0–,0.5 | 0.02 to 0.4 |
| Tantalum | 0-1 | 0.01 to 0.10 |
| Tin | 0–,4 | 0.02 to 3.0 |
| Tungsten | 0-5 | 0.01 to -0.10 |
| Vanadium | 0–,15 | 0.01 to 15.0 |
| Yttrium | 0–,0.04 | 0.001 to 0.004 |
| Zirconium | 0–,5 | 0.003 to 4.0 |