ASTM D876-13 + Redline

ASTM D876-13 + Redline

Standard Test Methods for Nonrigid Vinyl Chloride Polymer Tubing Used for Electrical Insulation

More details

Download

PDF AVAILABLE FORMATS IMMEDIATE DOWNLOAD
$30.00

$60.00

(price reduced by 50 %)

1.1 ,These test methods cover the testing of general-purpose (Grade A), low-temperature (Grade B), and high-temperature (Grade C)2 nonrigid vinyl chloride polymer tubing, or its copolymers with other materials, for use as electrical insulation. For the purpose of these test methods nonrigid tubing shall be tubing having an initial elongation in excess of 100 ,% at break.

Note 1—,These test methods are similar but not identical to those in IEC 60684–,2.