Standard Practice for Recovery of Emulsified Asphalt Residue Using a Vacuum Oven

More details

Download

PDF AVAILABLE FORMATS IMMEDIATE DOWNLOAD
$22.50

$45.00

(price reduced by 50 %)

1.1 ,This practice is suitable for recovery of the residue of emulsified asphalts composed principally of a semisolid or liquid asphaltic base, water and an emulsifying agent. Asphalt base may be pre-modified with polymeric modifiers or latex polymer modifiers may be incorporated into the emulsified asphalt through co-milling or post emulsified asphalt production blending.