1.1 ,These test methods explain the use of the shearing disk viscometer to obtain an indication of the processability of non-pigmented emulsion styrene-butadiene rubbers (SBR). The test methods described should not be used to compare processability characteristics of polymers that produce a test curve significantly different from that shown in Fig. 1.
FIG. 1 ,Typical Mooney versus Time Curve for Processability Test of SBR