ASTM D3826-18 + Redline

ASTM D3826-18 + Redline

Standard Practice for Determining Degradation End Point in Degradable Polyethylene and Polypropylene Using a Tensile Test

More details

Download

PDF AVAILABLE FORMATS IMMEDIATE DOWNLOAD
$23.50

$47.00

(price reduced by 50 %)

1.1 ,This practice covers the determination of a degradation-end point (a brittle point) for degradable polyethylene/polypropylene films and sheeting less than 1.0 mm (0.04 in.) thick. This practice is not intended for determination of the rate or degree of degradation of a polyethylene/polypropylene film or sheet, but rather, to assess when in the course of its degradation under some condition, a brittle point is reached. If one wishes to monitor tensile elongation during the degradation process (such as when the tensile elongation is significantly greater than 5 ,%), Test Method D882 is recommended. This practice is not to be considered the only way of determining a degradation-end point.

Contact us