1.1 ,This test method covers an accelerated exposure test intended to simulate defects in automotive clearcoats caused by acid rain2 that occur at the Jacksonville, Florida exposure site. Exterior exposures at an acid rain test location in Jacksonville, Florida produce etch defects that range from small pits to 12.7 mm [0.5 in.] in diameter or larger acid-etched spots. The latter type of defect is not produced in other acid-etch tests that only produce pits that are smaller than 6.35 mm [0.25 in.] in diameter.3
Note 1: ,Digital images of the acid etch defects produced in outdoor acid-rain exposures and in the accelerated test described in this test method are found in Appendix X1.