1.1 ,This practice covers techniques to accelerate weathering effects of factory-coated embossed hardboard using Cycle 1 of Practice G90 (concentrated natural sunlight with periodic surface water spray) plus a soak-freeze thaw cycle (see Section 5 of this practice).